Table of Contents
- What is doming on a logo?
- Which resin should I choose for a domed logo?
- Which substrates can a domed logo be applied to?
- How do I prepare a logo for resin coating?
- How do I produce and inspect domed logos?
- Frequently Asked Questions
Doming consists of applying a transparent, raised resin onto a previously printed visual. The choice of resin, substrate, and adhesive, along with the preparation of the graphic file, are all factors that determine the quality of your custom 3D stickers and how well they suit your equipment.
What is doming on a logo?
Doming does not print the logo: it covers it after printing. This marking technique gives the visual a relief that is both visible to the eye and perceptible to the touch.

The principle of the domed label
A liquid resin is deposited onto a previously printed and cut logo. As it hardens, it forms a convex relief that gives the visual its domed appearance. It is a finish applied after printing, not 3D printing. A self-adhesive domed label generally consists of three elements: a printed substrate, a layer of transparent resin, and an adhesive.
When the resin dome is transparent, the logo remains visible while benefiting from a sense of depth and a relief that is perceptible both to the eye and to the touch. The terms 3D sticker , 3D resin sticker and raised label often refer to this same process.
Relief compared with other markings
Doming creates a magnifying-glass effect that highlights the logo. Its smooth, glossy surface also helps protect the print against superficial scratches and moisture. Conversely, a flat-printed marking avoids adding thickness and the resin step, but it offers neither the same visual effect nor the same feel or level of protection for the printed surface.
Pad printing and digital transfer make it possible to reproduce a visual directly onto an object. However, these processes alone do not create a protective transparent dome. To achieve this relief effect, Thermoflan offers polyurethane and UV doming solutions, which differ notably in their curing method.
Which resin should I choose for a domed logo?
The choice of resin determines production speed, aesthetic result, and how well the logo holds up over time. Thermoflan helps you choose between UV doming and polyurethane, depending on your productivity goals and the constraints of the end use. The nature of the resin, the desired finish, and the actual exposure conditions are all criteria to consider when selecting the most suitable solution.

Polyurethane, UV and other families
Thermoflan offers two technologies for adding relief to a logo. The first is based on a polyurethane resin combined with a hardener, which must be cured in an oven. The second uses a resin that hardens under ultraviolet (UV) lamps. The choice between these two processes depends mainly on the logo’s exposure conditions, the production volumes, and the manufacturing lead times.
- Polyurethane resin: offered in flexible and semi-rigid versions, it is presented by Thermoflan as suitable for logos exposed to bad weather, UV, or intensive use. Its curing requires passing through an oven.
- Flexible UV resin: it is aimed in particular at small and medium runs and at production with short lead times. The term “UV” here refers to the curing method, not necessarily an acrylic resin.
- Standard epoxy: it can yellow and become brittle under UV. Thermoflan does not offer epoxy technology in its doming range.
Between polyurethane and epoxy resin, the difference therefore lies in their behavior under UV, as described in the list.
| Technology | Curing | Versions | Uses cited by Thermoflan |
| Polyurethane | Resin + hardener + oven | Flexible, semi-rigid | Bad weather, UV, intensive use |
| UV | Resin + hardener + ultraviolet lamps | Flexible | Small or medium runs, short lead times |
| Epoxy | Not offered by Thermoflan | — | May yellow and become brittle under UV exposure |
When lead time is the priority, UV resin that cures under lamps more easily suits short runs.
Transparency, finish and height
A clear resin preserves the visibility of colors and details in the printed artwork. The glossy look results from the smooth surface of the cured resin, which reflects light, whereas a matte finish diffuses reflections more. To choose the right formulation, several criteria must be considered: transparency, risk of yellowing, adhesion to the print, UV resistance, and the hardness or flexibility obtained after curing.
The height of the raised relief depends on several parameters, including the label format, its outline and the resin formulation. Some manufacturing guides indicate heights between 1.5 and 3 mm depending on the part. This range is indicative only and is not a guaranteed dimension for all logos. The achievable height must be validated based on the artwork’s geometry and the manufacturing characteristics.
Real-world performance in outdoor use
Outdoors, the durability of a domed label depends on all of its components: resin, inks, face material and adhesive. It also varies with exposure and use conditions: climate, orientation, humidity, cleaning, abrasion and temperature variations.
For polyurethane resin, the Thermoflan technical data sheet indicates 8 years of resistance to UV, outdoor exposure and chemicals. However, this figure concerns the resin alone and does not constitute a service life guarantee for the complete label.
UV protection and chemical resistance therefore depend on the formulation and actual exposure conditions. The ISO 4892-1:2024 standard governs laboratory light-exposure testing. On its own, it does not convert test hours into years of outdoor exposure.
Which substrates can a domed logo be applied to?
A domed label relies on the combination of a printed face material, which receives the resin, and an adhesive that secures it to the final substrate. Choosing these two components is essential: the face material must provide good resin adhesion, while the adhesive must ensure durable attachment to the destination surface. They must therefore be selected based on the material, the shape of the part and the conditions of use of the logo.
Choosing the face material and its finish
The face material receives the print, then the resin. Several materials and finishes are possible:
- Vinyl and polyester films: common substrates for domed promotional stickers.
- Self-adhesive PVC and polypropylene: other face materials used for doming.
- Metallized substrates or coated papers: possible, subject to compatibility with the resin.
Available finishes include white, transparent, metallic and brushed aluminum look. Check the compatibility of the resin with the actual face material surface, taking into account the ink and any varnish. The polyurethane resin offered by Thermoflan in particular requires a non-porous surface to prevent material seepage and bubble formation.
Matching the adhesive to the final part
A permanent, repositionable or reinforced adhesive can be chosen depending on the material and roughness of the part, temperatures, humidity and the desired bonding duration. Polyethylene and polypropylene, which have low surface energy, require a suitable adhesive and a test on the actual part.
The NF EN ISO 29862:2024 standard describes, among other things, a 180° peel test. However, this measurement does not replace an application test on the final substrate. According to a European guide, most standard adhesives require an application temperature of at least +5 °C. Their service range can extend from −40 to +80 °C, although these values do not apply to all domed logos.
Professional uses and application conditions
The domed logo finds its place on many substrates: automotive badges and emblems, electronic devices, nameplates, industrial equipment or promotional items. The application surface should ideally be flat and rigid. For a resin magnet, the artwork printed on a magnetic sheet is covered with a translucent resin that gives it relief. On a machine, a piece of furniture or a vehicle, the substrate must be compatible with the adhesive, clean and dry.
How to prepare a logo for resin coating?
The magnifying effect of the resin highlights the qualities of the visual, but also accentuates its flaws. Preparing the logo rests on three essential points: defining the contour, preparing the print file, and the checks to carry out before production starts.
Shape and die-cut contour
The contour determines the area where the resin stops. Thermoflan recommends favouring rounded shapes to obtain an even dome.
- Recommended shapes: circles, ovals, squares and rectangles with rounded corners, which allow the resin to stop evenly.
- High-risk shapes: points, narrow necks and very fine details, which increase the risk of overflow or insufficient material.
- Custom shapes: these require a vectorised cutting path. The flow of the resin may, however, slightly round the corners.
Characters and fine lines must also be checked at their final size. The magnifying effect of the resin can indeed accentuate defects in the visual once the logo is domed.
File, colours and printing
A vector file is preferred to guarantee the sharpness of the logo. For a raster image, a resolution of 300 dpi minimum at final size is recommended. Convert the visual to CMYK, the printing mode, rather than RGB, which is intended for screens. A logo printed in four-colour process reproduces gradients, but on its own does not guarantee an exactly identical Pantone colour.
The printing process may be digital, offset, UV or screen printing, depending on the medium used. Water-based inks should be avoided. In all cases, the inks must adhere well to the medium and be perfectly dry before the resin is applied, to ensure their compatibility with doming.
Items to validate before production
A technical sheet dedicated to doming recommends 2 mm of bleed and a 2 mm safety margin. These values must, however, be confirmed with the chosen workshop.
The file submitted for validation must show the visual at its final size, the cutting contour, the colours, the finish and the version of the logo. Fonts must be embedded or converted to outlines to avoid any substitution when the file is opened on another workstation.
How to produce and check domed logos?
Production takes place in three stages: preparing the boards, applying the resin, then checking and receiving the batches. At each stage, the consistency of the relief depends on the precision of the settings and on control of the production conditions.
Preparing the boards and equipment
Half-cut (kiss-cut) die-cutting outlines the doming labels without cutting through the liner, the lower backing. Weeding then consists of removing the excess film without lifting the edges of the labels being kept. Thermoflan recommends clean, flat boards, ideally in A4 format, with at least 1 mm spacing between the labels.
- Polyurethane setup: resin and hardener, mixer-degasser, pneumatic applicator, drying trays and oven for heat curing.
- UV setup: semi-automatic applicator and UVA curing oven, whose lamps cure the deposited resin.
- Mixer-degasser: it homogenises the polyurethane resin and its hardener, then removes the air bubbles trapped in the mixture.
The choice of equipment depends on the resin selected, as mentioned above. For polyurethane, the polyurethane doming line is organised around the mixer-degasser, the applicator and the oven, which is essential for curing.
Dosing, depositing and curing
Thanks to surface tension, the resin stays contained within the edges of the label. Regular dosing produces an even dome, whereas an excess of material risks causing overflows.
For its polyurethane resin, Thermoflan indicates a consumption of about 1 g of mixture per 5 to 6 cm², or roughly 1.7 to 2 kg/m² for a 1.8 mm dome. These values remain indicative and must be adjusted to the geometry of the label. The resin and hardener are mixed at a 1:1 ratio and must be applied within approximately 15 to 20 minutes, depending on temperature. This dosage does not necessarily apply to other formulations.
Curing then determines the hardness and gloss of the dome. For its polyurethane resin, Thermoflan specifies 6 hours in an oven at 40 °C. Another source mentions curing for about 24 hours at room temperature. For this process, it is recommended to keep the workshop above 20 °C and relative humidity below 60%.
Defects, receiving and safety
At final inspection, the dome must show uniform transparency and relief. Check for bubbles, craters, dust, runs, resin shortfalls and insufficiently cured areas. If a defect appears, check the dosage, the mixing, the flatness of the plates and the compatibility of the different layers.
To compare quotes, the specification must state the resin-coated area, dimensions, distinct visuals and quantities. It must also define the front face, adhesive, resin, finish and packaging. The approved proof and reference sample then make it easier to check goods on receipt. ISO 2859-1:2026 describes sampling plans for attribute inspection, but on its own does not define the acceptable defects for a lot.
Before any resin application, consult the safety data sheet of each component. Since 24 August 2023, the Regulation (EU) 2020/1149 on diisocyanates requires prior training for professionals using products containing at least 0.1% by weight of diisocyanates. This threshold applies to the total diisocyanate content of the product.

Equip your workshop for logo doming
Polyurethane or UV resin, applicator, trays and ovens: Thermoflan helps professionals add relief to their logos.
Frequently asked questions
Which resin should I choose to apply a domed logo on a curved surface?
Thermoflan recommends a flexible resin for curved surfaces. However, 3D stickers are mainly designed for smooth, clean and dry surfaces. A curved, flexible part that has been recently painted or textured therefore requires special checking before any series application.
Why does the resin spill over the edge of the label during doming?
The overflow may be caused by the dosage, the cutting contour, the flatness of the sheet or the flow of the resin. Thermoflan also recommends adjusting the cutting pressure so that it cuts only through the vinyl, without damaging the liner.
Why does a domed logo peel off after application?
Peeling may result from an unsuitable adhesive, a damp or greasy surface, or insufficient application pressure. The surface must be clean and dry. Avoid touching or stretching the adhesive and apply even pressure during application. If the resin is peeling from the graphic, the problem may come from insufficiently cured ink, contamination, or incompatibility between the different layers.